STOa101005S2

SrTiO3 (100) 10x10x0.5 mm Epi polished wafer, 2SP - STOa101005S2

SrTiO3 single crystal provides a good lattice match to most materials with a perovskite structure. MTI has a full production line for manufacturing high-purity SrTiO3 powder, single crystal boules, and EPI-polished substrates in many sizes.

SrTiO3 single crystal provides a good lattice match to most materials with a perovskite structure. It is an excellent substrate for epitaxial growth of HTS and many oxide thin films. SrTiO3 single crystal is also widely used for special optical windows and as a high-quality sputtering target.

MTI has a full production line for manufacturing high-purity SrTiO3 powder, single crystal boules, and EPI-polished substrates in many sizes.

Request a quote
  • Substrate: SrTiO3
  • Size: 10 × 10 × 0.5 mm ±0.05 mm (1.0 mm thickness available as an option)
  • Orientation: (100) ±0.5°
  • Edge Orientation Indication: <001> ±2° available as an option
  • Polish: EPI polished by CMP technology with reduced sub-surface lattice damage
  • Surface Finish (RMS or Ra): <5 Å
  • Package: Class 100 plastic bag under Class 1000 clean room conditions

Typical Physical Properties

Crystal Structure Cubic, a = 3.905 Å
Growth Method Verneuil
Density 5.175 g/cm3
Melting Point 2080°C
Hardness 6 (Mohs)
Thermal Expansion 10.4 × 10-6/°C
Dielectric Constant ~300
Loss Tangent at 10 GHz ~5 × 10-4 @ 300 K, ~3 × 10-4 @ 77 K
Color and Appearance Transparent; sometimes slightly brown depending on annealing conditions. No twins.
Chemical Stability Insoluble in water

Note: SrTiO3 is grown by the Verneuil flame-fusion method. Crystal perfection may therefore vary between substrates, and the rocking curve may differ from substrate to substrate. Please inspect the SrTiO3 substrate before growth.

XRD is not routinely performed on every substrate in order to keep costs low. If rocking-curve measurement is required, please request it before ordering. Additional charges may apply.

SrTiO3 crystal boule SrTiO3 Verneuil growth process SrTiO3 Verneuil crystal growth