STOa101005S1StepUS

SrTiO3 Substrate with Step Surface & Ti terminated (100) 10x10x0.5mm, 1 SP - STOa101005S1StepUS

Homoepitaxy of SrTiO3 film on the crystal surface proceeds in a layer-by-layer mode, as verified by reflection high-energy electron diffraction and atomic force microscopy. Step SrTiO3 Substrate is an atomically smooth SrTiO3 (100) substrate with steps one unit cell in height, obtained by treating the crystal surface with a pH-controlled NH4F-HF solution.

Step SrTiO3 Substrate is an atomically smooth SrTiO3 (100) substrate with steps one unit cell in height, obtained by treating the crystal surface with a pH-controlled NH4F-HF solution.

Homoepitaxy of SrTiO3 film on the crystal surface proceeds in a layer-by-layer mode, as verified by reflection high-energy electron diffraction and atomic force microscopy. Ion scattering spectroscopy revealed that the TiO2 atomic plane terminates the as-treated clean surface and that the terminating atomic layer can be tuned to the SrO atomic plane by homoepitaxial growth. This technology provides a well-defined substrate surface for atomically regulated epitaxial growth of perovskite oxide films.

For more information on Step substrates, please refer to: Science, 2 December 1994, Vol. 266, No. 5190, pp. 1540–1542, DOI: 10.1126/science.266.5190.1540

Request a quote
AFM image of SrTiO3 substrate after Step treatment
Surface of SrTiO3 substrate after Step treatment (AFM)
AFM image of SrTiO3 substrate before Step treatment
Surface of SrTiO3 substrate before Step treatment (AFM)
Typical AFM image of Step SrTiO3 substrate
Typical AFM image of Step SrTiO3 substrate

  • Size: 10 × 10 × 0.5 mm ±0.05 mm
  • Orientation: 0.1° miscut from (100) (±0.1° from Y and X directions)
  • Polish: One side EPI polished by CMP technology with less sub-surface lattice damage
  • Surface Termination: TiO2 layer via special etching
  • Surface Finish (RMS or Ra): <5 Å

Typical Physical Properties

Crystal Structure Cubic, a = 3.905 Å
Growth Method Verneuil
Density 5.175 g/cm3
Melting Point 2080°C
Hardness 6 Mohs
Thermal Expansion 10.4 × 10-6/°C
Dielectric Constant ~300
Loss Tangent at 10 GHz ~5 × 10-4 @ 300 K, ~3 × 10-4 @ 77 K
Color and Appearance Transparent, sometimes slightly brown depending on annealing conditions; no twins
Chemical Stability Insoluble in water