Physical Properties |
||
|
|
D10 (μm) |
|
|
D50 (μm) |
|
|
|
D90 (μm) |
|
|
|
Powder Appearance |
|
|
|
Tap Density (g/cm3) |
|
|
|
Specific Surface Area (m2/g) |
|
|
|
Moisture (ppm) |
|
|
|
Discharge Capacity (mAh/g) |
|
|
|
Coulombic Efficiency (%) |
|
|
|
SDS |
|
|
|
Note: MTI does not manufacture this product, and only sells a small quantity to research the development of new-generation battery. |
||
Application Notes:
- Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
- Please keep the powder in the vacuum box to avoid moisture.
- Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max capacity.