Size: 2" Dia. +/-0.5 mm x 0.5 mm +/-0.05 mm
Orientation: <100> +/-0.5 Deg
Surface Roughness: CMP polished with min. sub-surface damage , and Ra < 10 A
Package: Packing in 1000 class clean room with 100 grade clean plastic bag
|
Typical Physical Properties |
Chemical Formula |
( LaAlO3)0.3 (Sr2AlTaO6)0.7 or ( La0.18Sr0.82)(Al0.59Ta0.41)O3 |
Crystal Structure |
cubic: a = 3.868 Å |
Growth Method |
Czochralski |
Density |
6.74 g/cm3 |
Melt Point |
1840 oC |
Thermal expansion |
10 (x10-6/ oC) |
Dielectric Constant |
~ 22 |
Color and Appearance |
Colorless to light brown based on annealing condition. |
Standard Products | |
|
Epi -polished substrates <100>ori. ± 0.5o 1or 2 sides polished Ra < 8 Å |
10 x 10 x 0.5mm Special size and orientation is available upon request 5 x 5 x 0.5 mm |