- Orientation: (100) ±0.5°
- Size: 5 × 5 × 0.5 mm
- Polish: Two sides optical-grade polished
- Surface Finish (RMS or Ra): < 5 Å
- Packing: Each substrate packed in a membrane box
Please click here to see the KTN crystal rocking curve
Please click here to see a typical AFM image of the KTN substrate

Typical Properties
| Chemistry | KTa1-xNbxO3, x ≈ 0.33 |
| Crystal Growth Method | Top-seed flux growth |
| Crystal Structure | Cubic, Perovskite; a = 3.990 Å |
| Melting Point | Does not melt congruently |
| Curie Temperature | 20–30°C |
| Density | 7.015 g/cm3 |
| Thermal Conductivity | 0.17 W/(m·K) at 300 K |
| Linear Electro-Optical Coefficient | r33 > 600 pm/V |
| Refractive Index | 2.234 |
| Coercive Field | Ec = 250 V/mm |
| Transmission Range | 400–4000 nm |