| Model |
HC-025D |
HC-05D |
HC-075D |
HC-15D |
HC-30D |
Product structures
|
Including one set of 0.25"(I.D.) Dry Pressing Die: 6 metric Ton Max Load.
|
Including one set of 0.5" ( I.D. ) Pressing Die: 10 metric Ton Max Load.
|
Including one set of 0.75" (I.D.) Pressing Die: 12 metric Ton Max Load.
|
Including one set of 1.5" ( I.D. ) Pressing Die: 16 metric Ton Max Load.
|
Including one set of 3.0"( I.D.) Pressing Die: 16 Ton Max Load.
|
Product Dimensions
|
|
|
|
|
|
| Hardness |
> HRC 60 |
| Roughness Average (Ra) |
0.08 μm |
| Voltage |
- AC 220V 50/60Hz (To use AC 110V, please order a 500W transformer )
- 220V AC Power plug is not included. Please click here to order the plug)
|
| Working Temperature Range |
50-280 ºC |
Temputerature Control Method
|
- Single-point digital temperature controller
- Type-K thermocouple
|
Steps to Make Sample Pellet |
- Mixing and grinding chemical powder by agate mortar or Ball Mill.
- Calcine mixed the powder in a high temp furnace under a suitable temperature.
- Crushing and Grinding calcined powder again by mortar or ball mill.
- Put calcined powder into the die.
- Pressing sample by a pressing machine under suitable pressure.
- Take out pellet samples from the die.
- Sintering the pellet under a suitable temperature.
- The sample is ready.
|
Cautions
|
-
Please consider using the 3'' Dia. Sieve Set No.200&450 Mesh to separate the 32~75 microns particles from the powder clumps. Please clean the mold via ethanol after the completion of each experiment.
- Please use ethanol to clean the pressing die every time before use.
- Store it in a dry environment with antirust oil after the operation to avoid rusting. No warranty for rushing.
- For pressing sticky metal powders such as Al, Mg, Zn, it is necessary to use dry or alcohol-based tool lubricant to lubricate the die and sleeve set to reduce friction during the compression.
-
You may consider using BN coating (BNMR) for easy mold release. Please click the picture below to order.
|