FmSi3N4onSiBa100D0525C1FT100

100 nm Silicon Nitride Film (PE-CVD) on Si(100) P-type, B-doped 100 mm dia x0.525mm thick, 1sp, R:0.001-0.005 ohm.cm - FmSi3N4onSiBa100D0525C1FT100

Si3N4 Film coated by low stress PE-CVD method. Si3N4 Thickness: 100nm +/- 8%. Packing: Vacuum packed on a 4" single wafer carrier box Optional: You may order: Optional: Precision Manual Diamond Wafer Scriber for Wafer dicing.

Silicon Nitride Film

  • Si3N4 Film coated by low stress PE-CVD method
  • Si3N4 Thickness:   100nm  +/- 8%
  • Si3N4 covers front polished side of Silicon wafer ONLY
  • Refractive Index of Si3N3: 1.98 +/-0.05 @ 632.8nm

Silicon Wafer Specifications:

  • Conductive type:        Si P- type, B-doped
  • Resistivity:                 0.001-0.005 ohm-cm
  • Size:                          4" diameter +/- 0.5 mm x 0.525 +/- 0.025 mm th
  • Orientation:                (100) +/- 0.5o
  • Polish:                        One side polished
  • Surface roughness:     Prime
  • Packing:                      Vacuum packed on a 4" single wafer carrier box