FmAlNonALc101005S1FT1000US

Undoped AlN Template on Sapphire(0001)

AlN Template on sapphire (10x10mmx1000nm) is made by a Plasma Vapor Deposition of NanoColumns (PVDNC)-based method. Surface Rughness and XRD data.

AlN Template on sapphire (10x10mmx1000nm) is made by a Plasma Vapor Deposition of NanoColumns (PVDNC)-based method. AlN template is a cost effective way to replace AlN single crystal substrate.

Request a quote
 Size 10mmx10mm
Substrate Sapphire Orientation c axis (0001) +/- 1.0 deg.
Type and Doping for the AlN film Undoped, Semi-insulating
Macro Defect Density <5 cm-2
Front Surface Finish (Al Face) As-grown
Back Surface Finish Sapphire as-received finish
Useable Surface Area >90% 
Edge Exclusion Area 1mm
Package Single Wafer Container
AlN layer thickness 1000 nm +/- 5%
 