Fm300SOonSIBa100D05C1R001US

Thermal Oxide Wafer: 300 nm SiO2 Layer on Si (100), 100mm dia x 0.5 mm t, P type, 1SP R:0.01-0.05 ohm.cm - Fm300SOonSIBa100D05C1R001US

Home›Crystals›Thin Films A-Z›Silica on Silicon(Thermal Oxide Wafer)›Fm300SOonSIBa100D05C1R001US. Thermal oxide Research Grade, about 80 % useful area.

Thermal oxide 

Research Grade, about 80 % useful area

  • SiO2 layer on 100mm Silicon wafer
  • Oxide layer thickness: 300 nm ( 3000A) +/- 10%
  • Refractive index - 1.455

Silicon Wafer Specifications:

  • Conductive type: P-type/ B-doped
  • Resistivity: 0.01-0.05 ohm.cm (If you would like to measure the resistivity accurately, 
    please order our Portable 4 Probe Resistivity Testing Instrument.) 
  • Size: 100mm dia +/- 0.5 mm x 0.5 mm th
  • Orientation: (100) +/- 0.5o
  • Polish: one side polished
  • Surface roughness, Ra: < 5A (RMS)

 

Request a quote