Fm300SOonSIBa100D05C1R0001
Thermal Oxide Wafer: 300nm SiO2 Layer on Si (100)100mm diax0.5 mm t, P type, 1SP R:0.001-0.005 ohm.cm - Fm300SOonSIBa100D05C1R0001
Home›Crystals›Thin Films A-Z›Silica on Silicon(Thermal Oxide Wafer)›Fm300SOonSIBa100D05C1R0001. Research Grade, about 80% useful area.
Thermal oxide Layer
-
Research Grade, about 80% useful area
- SiO2 layer on 100mm Silicon wafer
- Oxide layer thickness: 300 nm (3000A) +/-10%
- Refractive index - 1.455
Silicon Wafer Specifications:
- Conductive type: P-type/ B-doped
- Resistivity: R:0.001-0.005ohm.cm (If you would like to measure the resistivity accurately,
please order our Portable 4 Probe Resistivity Testing Instrument.) - Size: 100mm+/- 0.5 mm x 0.5 mm
- Orientation: (100) +/- 0.5o
- Polish: one side polished
- Surface roughness, Ra: < 5A (RMS)