| Material |
- 7075 Aluminium alloy
- Tensile Strength: 524MPa
- 0.2% Yield strength: 455MPa
- Hardness: 150HB
- Max. working temperature 150oC
|
| Well Options, dimension, and Max. load |
- 9 wells and 25 wells are standard products,
- Please choose from the product option bar
- The customized well number is available upon request at an extra cost
- Max. pressure for single well: 90 MPa
- 9 Well die: L50mm*W50mm*H30mm 6.3 metric tons
- 16 well die: L60mm*W60mm*H30mm 11.2 metric tons
- 25 well die: L75mm*W*75mm*H30mm 18 metric tons
- 36 well die: L90mm*W90mm*H30mm (25 metric tons
- 48 well die L133mm*W100mm*H30 mm (33.6 metric tons)
|
| Related High throughput Device |
- May choose MSK-SFM-50 plate shaker as HTP mixer ( Click Pic 1 to order )
- May use YLJ-HP300 the flat hot press to press multi-well die ( Pic. 2)
- Please use XRF-32-LD for automatic composition analysis by the XRF scanning system ( Click Pic. 3
Pic. 1 Pic. 2 Pic. 3
|
Cautions
|
- WARNING:
-
DO NOT press flammable, corrosive, or explosive materials
- Attention:
- To achieve the best result, please ensure the volume of sample powder in all 32 pressing dies are the same.
- Use ethanol to clean the pressing die before and after use every time
- Use anti-rust oil after the operation and store it in a dry place to avoid rusting.
-
3'' Dia. Sieve Set No.200&450 Mesh can be used to separate the 32~75 microns particles from the powder clumps
- .
|
Steps to make a sample pellet |
- Mixing and grinding chemical powder by agate mortar or Ball Mill
- Calcine mixed the powder in a high temp furnace under a suitable temperature
- Crushing and Grinding calcined powder again by mortar or ball mill
- Put calcined powder into the die
- Pressing sample by a pressing machine under suitable pressure
- Take out the pellet sample from die
- Sintering the pellet under a suitable temperature in Oven
- Then, a new material sample is formed!
|